TPSIV回收|3C包胶料呆滞了别当硅胶卖,科隆新材分级消化把死钱变活钱

塑料知识科普 发布时间: 2026-09-15 1583 阅读

Old Luo is doing phone mid-frame coating in Shenzhen, and the two TPSiV 3451-80A pallets in the warehouse have been sitting on trays for almost half a year. A phone solution provider modified the coating material, and the inventory of TPSIV pellets suddenly increased by two to three tons. The bags were still sealed fine, but the warehouse manager checked the ledger and found the unit price wasn't cheap—one ton was worth three tons of ordinary TPE. Old Luo squatted at the workshop door to calculate the accounts: TPSIV emphasizes low precipitation; after sitting for a while, a layer of siloxane leach appears on the surface, and when wrapped on the mid-frame, it wastes easily. 3C customers simply don't accept it.

Obsolete material isn't an asset, it's a liability lying on the books.

TPSIV this stuff, only bosses who make phone rubber-coated devices, wearable watch straps, and low-release buttons are familiar with this. It's a vulcanized thermoplastic blended with siloxane and elastomer, with a smooth feel, low weather resistance, and low precipitation, but it's much more expensive. The problem is it's sensitive to storage conditions—when the temperature rises, it slowly forms on the surface, and after absorbing moisture, the injection molding fogs up. What's even more troublesome is that hardness levels are 65A, 70A, and 80A, corresponding to different phone frames. Sellers don't even distinguish between them—one ton is like a ton per ton. TPSIV leaching is like a sweaty fingerprint on a new computer's surface—it doesn't look serious, and you can't even wipe it off.

The essence of recycling isn't selling scrap, but turning dead money into living money.

Let me tell a real story. A boss called in a bulk supplier, who pinched a TPSIV tablet and rubbed it, said it was oily or excessive, and charged at floor price. The wholesaler's calculations are even more sophisticated than your accountant's—he takes them back and mixes them into low-end daily necessities, adds some filler when the sediment is large, and the keys they make become sticky after just two months, with all the price difference going into their pockets. Think about it, what he says doesn't work—it's not that he really has no customers, but that he doesn't have any 3C customers himself. Some vendors are even worse, not even testing hardness, mixing 70A and 80A into a truckload.

Consolidated goods dealers aren't helping you deal with scrap; they're using your good materials to cover their subpar parts.

Kelong New Materials is taking the path of terminal digestion. We have long-term downstream customers specializing in 3C overmolding, wearables, and low-degradation parts. For grades like TPSiV 3451-80A, which have limited circulation but stable demand, we can buy them in that match the customer's formula and ship directly without inventory pressure. If the batch is slightly off, we can digest it into our own modified formula system, regardless of hardness or batch. Pricing is based on Shore hardness, precipitation amount, and tensile strength, with one price per grade, clearly stated on the recall form. With our own production capacity and customer backing, our prices are stable and don't fluctuate with market trends.

Good material isn't afraid of not being picked up; what's scary is selling good material as scrap.

On the day of the on-site evaluation, our technician brought a Shore hardness tester and a rapid surface precipitation tester to measure hardness and check for siloxane emissions on site. You were present and weighed; the tare weight, gross weight, and net weight matched the three orders. Since TPSIV is expensive, we create separate records, recording 70A and 80A separately, not using the wholesale price for a single purchase.

A different approach is more cost-effective—replace recycled material with new material. Process five steps: first report materials, take photos, specify grade, tonnage, and city; We conduct on-site graded evaluations and quote on the spot after testing; On-site weighing and receiving goods; Payment directly offset your purchase of new material from Cologne; Final settlement and invoice. A long-term customer who makes watch bands stored about 2 tons of obsolete TPSIV material in their warehouse, which offset nearly half of the new material payment by grading, saving about 20,000 yuan in cash flow. The newly brought back products are the full range of QUANICE elastomers, which are directly added to the production line for renewal.

To put it bluntly, scrap isn't something you can't accept; it depends on how you handle it.

As for specific grades, we regularly recycle mainstream grades like Dow (formerly Dow Corning) TPSiV 4000-70A, TPSiV 3451-80A, TPSiV 3345-65A, and Dawn TPSIV; Domestic substitution grades like Zhejiang Zhonggao and Ningbo Keyuan are subject to physical appraisal. Recyclable forms include obsolete original packaging (whole or loose packs), phone frame glue sprue materials, watch strap gate materials, pelletizer head materials, scrap parts, and inventory scraps. Severe precipitation particles should be sampled separately; don't mix them with new pellets in the same bag.

To be honest, TPSIV is expensive, and 3C customers pick out precipitates. If you keep them in the warehouse and secretly use them, if the precipitation exceeds the standard and the flow reaches the customer, the loss is not just a small amount. It's better to find someone familiar with 3C parts while the quota is still up, and take it away in grading.

Just a quick chat to avoid pitfalls. Is recycling just selling cheap? The truth is selling by hardness and grading; good materials can be sold at good prices. No one wants high-end materials? The truth is finding the right end customers; both 3C and wearable factories are looking for suppliers. Who bids the higher price? The truth is, they bargain, weigh down, and delay payment when they get it, and the price is even worse than the three companies