Every spring and the start of the hottest period, factories making EVA foam shoe materials start to have headaches: uneven bubble holes, honeycomb holes appear when cut open; poor rebound means a pair of soles flattened after two months of use; worse is photovoltaic film manufacturers, whose resin has slightly lower VA content, causing yellow edges and delamination when laminated components, and the entire cabinet of boards is pulled away.

Bosses caught up in a failed car often react first with "EVA material is no good." Essentially, it's not that the material is bad; the batch of material in hand is not produced with the same VA content or the same process. EVA has a few points difference in vinyl acetate (VA) content, but its performance is a completely different matter.

This article will thoroughly explain the skill of "determining the life and death of VA content" in EVA, three leading foreign manufacturers, and how to choose sub-brands .

VA elastomer that determines life and death

EVA ethylene-vinyl acetate copolymer. The difference from polyethylene is that ethylene contains copolymer vinyl acetate. Low VA content means it is more plastic and harder; When VA content is high, it becomes softer, more elastic, and stickier. Hot melt adhesives, foamed shoe materials, and photovoltaic encapsulation films all rely on it.

To put it bluntly, VA content is EVA's "temper knob": foamed shoe materials use medium to high VA for good rebound; Photovoltaic film uses specialized grades with high transparency and low precipitation, requiring extremely high light transmission and bonding. The global EVA resin market is fragmented, with several foreign giants leading the way in high value-added markets.

Sub-brand material: The source of the sub-brand material is

EVA still the same four-type type: starting and stopping starting and tail materials, grade switching transition materials, batch of VA content or melting index slightly exceeding standards due to process fluctuations, and secondary line tail material.

It is still original original polymerized particles, with molecular structure identical to the genuine brand, not recycled material re-pelletized. Clear boundaries:

TypeSourceQualityTypical Use
Genuine BrandOriginal Factory Standard BatchVA Content, Melting Index All CompliantPhotovoltaic Film, Medical Food Grade
SubbrandOriginal factory substandard batchSome indicators slightly deviated, substrate consistencyOrdinary foam, hot melt adhesive, low-end film
Reused/sprue materialProcessed scraps repelledAlready experienced once heat historyLow requirements products
Regenerated materialRecycled plastic pelletizingLarge performance fluctuationsLow-end filling

For EVA, the weakest secondary item is often VA content or melting fingers. For ordinary foamed shoe materials or hot melt granules, these are handled by floating machines; But for photovoltaic film that can last ten years without yellowing, the secondary brand must be used carefully.

Dow: The two companies behind the name ELVAX™

The first is Dow. Here's an industry trivia: the "DuPont Elvax" that old buyers talk about is now a brand under Dow Inc. ELVAX™ EVA copolymer is now operated by Dow, used for soft rebound in shoe soles and high-transparency bonding for photovoltaic packaging—these are its signature applications. Representative grades include ELVAX™ 250 (about 28% VA), 150, and 260 series.

Dow ELVAX secondary brand features: full grade, stable batch selection, secondary brand mostly focused on melting finger fine-tuning, making ordinary foaming and hot melt adhesive a smooth backup; photovoltaic grade has a high threshold for genuine branding, so secondary brands generally do not recommend direct module use.

ExxonMobil: Escorene™ Ultra has both ends

The second is ExxonMobil. Their EVA is part of the Escorene™ Ultra series, representing grades FL 00328 (about 27% VA) and UL 00018 (about 17.5% VA). One end is for photovoltaic packaging and greenhouse films, the other for hot melt adhesive and cable modification, with broad applications. ExxonMobil has long ranked among the top in global EVA resin market share.

Advantages of their sub-brand: VA content is clearly labeled, sub-brand mainly focuses on melting finger and additive fine-tuning, making mid- to low-end foam and adhesive masterbatches, with good performance.

Lotte Chemical: A regular in Korean foamed footwear materials

The third brand is Lotte Chemical. As a large Korean petrochemical integrated company, its EVA foam-grade grade is highly recognized in the shoe material, slippers, and sports goods sectors, with a global EVA market share around 9%, followed closely by LG Chem and SABIC.

Features of its sub-brand: Foam-grade grade is well-matched, with good foam uniformity and foundation. For general shoe materials and mats, the sub-brand is used to test formulas, with low cost pressure.

When choosing EVA secondary brands, check the VA before testing

Practical operation is just three steps. Let's talk about the VA content first. A common deviation with EVA secondary brands is vague VA content; foam factories test VA first and then mix ingredients, not based on old labels on the bag. Then it's about different uses. Ordinary foamed shoe materials and hot melt adhesive can be used as sub-brands; Photovoltaic film and medical food grade are honest and practical, genuine brands. Also, test the melting index. If the melting index is too different, you need to readjust the extrusion and foaming temperatures.

The packaging also shows large packages for volume and small packages for testing, so make sure to use the original factory packaging. In short: EVA's secondary brand is the genuine twin brother, but the VA content test form lacks a 'pass' mark—whether the brother can use it depends on whether what you make is worthy of him.

Cologne warehouse in stock | EVA original packaging

Main recommended brands: Dow, ExxonMobil, Rakuten Chemical

Main grades: ELVAX, Escorene Ultra

Packaging specifications: both large and small packages in stock

Warehouse stock is usually around 5000 tons: small sub-brand stock 800-1000 tons, sub-brand containerized 300-500 tons, large package/ton package stock 3500-3900 tons

supply guarantee: test before signing

Wuxi footwear materials: sub-brand reduces the defect rate of bubble cells from 6 % to 1%

share a case. In Wuxi, Jiangsu, a client specializing in EVA foam insoles and midsoles previously used mixed materials, with VA content floating each batch, uneven bubble hole removal and honeycomb defect rates at 6% year-round, with full batch rework during peak seasons. Later, they switched to imported EVA sub-brand materials, with VA content and melting index batches aligned, foaming process locked, foam defect rate reduced from 6% to below 1%, and rebound pass rate raised to 98%.

saved nearly 1,000 per ton of material, and the annual rework was enough to open a new line. This is the material selection account—EVA sub-brand and genuine are copolymers from the same batch, only missing a standard stamp, used in foam shoe materials with high VA tolerance, just to absorb the surplus. Ningbo Kelong New Materials Co., Ltd. has long been handling imported major factory sub-brand materials. They handle many cases like foam and adhesive film every year. In short, they help you settle on "VA stability and uniform bubble holes" before prototyping.

Seven key mnemonics: EVA secondary brands won't fail

1. Photovoltaic film, medical food grade—use genuine brands, don't gamble on secondary brands;

2. Foamed shoe materials, floor mats, hot melt adhesive—secondary brands can provide a safety net;

3. Test VA content first, don't trust old labels on bags;

4. If the melting index is too different, the process must be completely reset;

5. Dow ELVAX, Exxon, Escorene, Rakuten—first identify the factory;

6. Large packages run volume, small packages test machines, original factory packaging;

7. Every time VA floats by one point, the recipe must be recalculated

Final Few Sentences

EVA, this stuff, the VA content determines life or death, and it’s indispensable for both foaming and photovoltaics. Secondary material is not waste granules; it’s the original factory copolymer from the same high-pressure production line that just missed a single certification mark. Using it in foamed shoe materials and hot melt adhesives saves real money and ensures batch consistency.