美容仪手柄用什么TPE?拉丝不断,可能是料太软

应用领域 发布时间: 2026-09-16 4363 阅读

When you touch it, it feels sticky and strings. The beauty device was first criticized for its feel. The handle of the beauty device cannot resist skincare products and peels after three days.

Conclusion first: The beauty device handle feels good and is chemically bonded together.

The beauty device handle is the 'part that touches skincare products': lotion, serum, held every day.

The material should have a good hand feel, be chemically resistant, and not sticky — conclusion first: SEBS-based TPE is mainstream for beauty device handles; for high chemical resistance requirements, TPU or silicone composites are preferred.

The biggest pitfall of beauty device handles: continuous stringing may be due to the material being too soft. If the material is too soft, stringing becomes sticky — the balance of softness and hardness is key for the handle.

The beauty device handle is the part for experiencing it: stickiness and stringiness are sources of complaints. Choosing the right material makes the beauty device high-end—it's an experience part, don't skimp on material costs.

Why TPE doesn't pull fibers: feel can be adjusted, chemical resistance can be added

Reasons for using TPE for beauty device handles: adjustable texture, chemical resistance, high efficiency, controllable cost—together, these four make it suitable for beauty device handles.

The feel is key: non-slip grip. Benchmark sample blind test evaluation—feel is the experiential line of beauty devices.

Chemical resistance cannot be skipped: apply emulsion and serum every day. Include chemical resistance testing in the acceptance check—corrosion and stickiness are problems.

Test it by touching lotion: essence, hand sweat, cleaning

Skincare product working conditions: lotion and essence residues. Chemical resistance data must be tested—corrosion, that's the problem.

Hand sweat condition: holding by hand. Anti-slip data needs to be tested—slipping is all about experience.

Clean condition: wipe clean. Stain resistance data must be tested—scratches cause complaints.

SEBS or silicone: check if the handle feels sticky

DimensionSEBS baseSilicone
feelsoft and glutinoussoft and sticky
Chemical-resistantCan doGood
BrushedControllableLow
CostLowMedium-high
EfficiencyInjection moldingVulcanization
BatchStableStable

Table reading: Silicone is chemically resistant but expensive and sticky; SEBS-based is cheap and soft to the touch — mainstream handles are SEBS-based.

High-end chemical-resistant silicone composite, conventional SEBS-based — choose according to positioning.

Two pitfalls: material too soft, chemically fake-resistant

Pitfall 1: The material is too soft. If it feels sticky when drawn and the handle is hard to grip, it's too soft—balance between softness and hardness should be included in the acceptance criteria.

Pitfall 2: Falsely claiming chemical resistance. The report states chemical resistance, but in reality it corrodes — chemical resistance should be accepted based on actual testing.

Pitfall 3: Overlooking precipitation. High-temperature precipitation, handle becomes sticky — precipitation testing must be conducted.

Chemical Resistance Acceptance: Soaking Solution, Drawing, Delamination

Three questions: What sample is the texture benchmarked against, what medium is used for chemical resistance, and what is the hardness window? One test: Actual grip measurement—three questions and one test make the supplier's details clear.

Hardness testing should come first: if the wire drawing keeps breaking, the material may be too soft. Test the hardness window first, then discuss the feel—hardness is the skeleton of the handle.

Making sample retention a habit: retain samples for each batch, and test them batch by batch for tactile and chemical resistance. When changing materials for a batch, compare first before scaling up — stable batches lead to fewer customer complaints.

Don't blame the process for the handle brushing first. The material is on the softer side, and when the mold temperature rises, it sticks and pulls fibers during demolding. Check both the formula's hardness and the mold temperature, increase the hardness by one level, and the fibers will break cleanly.

Resistance to chemicals is based on soaking in a 'mixed medium,' not a single emulsion. Essences and makeup removers are applied alternately, and with high temperatures, passing at room temperature does not mean it will still pass an hour in hand.

Low-saturation, pearlescent colors are extremely picky about the base color; if the substrate is slightly yellow, no color can be adjusted correctly. First, print the color swatch to confirm the base color, then discuss mass production. Low-cost materials have more impurities, and the yield of color spots cannot be improved.

The number of surface impurities must strictly adhere to the standard. Beauty devices that are applied to the face and hands, any rough edges, logo bubbles, or color spots are flaws that affect the sense of high-end quality, which can only be achieved with pure base materials.

The material of the beauty device handle is a 'detail-oriented type': if the feel is slightly off, the sense of high-end quality drops a level. Lotion is most active and most corrosive at body temperature, so choose the material based on operating conditions, not room temperature.

Key Points Checklist for Acceptance of Beauty Device Handles

ProjectTest methodPassing line
Chemical-resistantSoaking in mixed mediaNon-corrosive
BrushedDemolding visual inspectionNo brushing
PrecipitationLeft at high temperatureSurface is clean
Surface qualityNumber of impurities≤ Standard
BatchThree rounds of random inspectionsData consistency

Common Problems and Solutions Table for Beauty Device Handles

PhenomenonReasonCountermeasure
BrushedThe material is relatively softIncrease hardness
stickyMedia corrosionReplace chemical-resistant material
DelaminationParameter OffsetAdjust mold temperature and hold pressure
Deckle edgeMold wearMold repair
colored dotBase material impuritiesChange to a pure base material

If the handle of the beauty device keeps getting stringy, first check if the material is too soft; it's not a mold problem. Soft materials stick to the mold and become stringy, workers using blades to pry it off can halve the output. Increasing the hardness by half a notch often solves the problem.

Handle skin-touch use, Shore A 30-40 soft and smooth like a pacifier to be skin-friendly. Sticky exudation looks cheap when applied to the face, use a low-migration formula with low exuding oil.

The peel strength of the coated handle should be tested for long-term holding; it counts only if it doesn't come off when soaked in sweat. Should not be pried off with nails, should not crack when bent, data varies by batch.

Cologne Customer Case: Mass Delamination of Coating, Reproduced Against Production Benchmark

A consumer electronics factory in Ma'anshan had mass delamination of coated beauty instrument handles, with a high rework rate. Cologne cooperated with on-site production debugging until yield stabilized, and the tactile rebound matched benchmark samples. Production debugging tackled delamination at the source—the coating issue, mostly due to not finding the right temperature and pressure window.

Summary

For selecting beauty instrument handles, balance softness and hardness first, test chemical resistance afterward, ensure draw consistency, and let the formula guide decisions.

"What material should be used for this part?"

This is the question we are asked most often, and also the one we most enjoy answering. Because the answer is never “pick the most expensive,” it is always “pick the most suitable.”

Ningbo Cologne New Materials Co., Ltd. produces modified thermoplastic elastomers, modified nylon (PA6 / PA66 / PA46 / PA11 / PA12 / PA6T / PA9T and nylon alloys), modified PPO / PPS, and also supplies nylon resins, secondary materials, and bulk materials from major chemical companies.

这台机器上的件,说下工况我帮你看看

报个件、说清温度和要过的认证,当天回你两三个能打的方案。电话微信同号,找到人就能聊。

打电话 18969817163发邮件询价