美容仪手柄用什么TPE?拉丝不断,可能是料太软

应用领域 发布时间: 2026-09-14 1319 阅读

When you touch it, it feels sticky and strings. The beauty device was first criticized for its feel. The handle of the beauty device cannot resist skincare products and peels after three days.

Conclusion first: The beauty device handle feels good and is chemically bonded together.

The beauty device handle is the 'part that touches skincare products': lotion, serum, held every day.

The material should have a good hand feel, be chemically resistant, and not be sticky — conclusion first: SEBS-based TPE is mainstream for beauty device handles; for high chemical resistance requirements, TPU or silicone composites are preferred.

The biggest pitfall of beauty device handles: continuous stringing may be due to the material being too soft. If the material is too soft, stringing becomes sticky — the balance of softness and hardness is key for the handle.

The handle of the beauty device is a trial component: stickiness and scratching are complaints. Choosing the right material makes the beauty device high-end — for trial components, don't skimp on materials.

Why TPE doesn't pull fibers: feel can be adjusted, chemical resistance can be increased

Reasons for using TPE in beauty device handles: adjustable texture, chemical resistance, high efficiency, controllable cost — all four together make it suitable for beauty device handles.

The feel is key: non-slip grip. Benchmark sample blind test evaluation—feel is the experiential line of beauty devices.

Chemical resistance cannot be skipped: apply emulsion and serum every day. Include chemical resistance testing in the acceptance check—corrosion and stickiness are problems.

Test it by touching lotion: essence, hand sweat, cleaning

Skincare product working conditions: lotion and essence residue. Chemical resistance data must be tested—corrosion, that's the problem.

Hand sweat condition: holding by hand. Anti-slip data needs to be tested—slipping, it's all about the experience.

Cleaning conditions: wipe clean. Stain resistance data must be tested—scratches cause complaints.

SEBS or silicone: check if the handle feels sticky

DimensionSEBS baseSilicone
feelsoft and glutinoussoft and sticky
Chemical-resistantCan doGood
BrushedControllableLow
CostLowMedium-high
EfficiencyInjection moldingVulcanization
BatchStableStable

Table reading: Silicone is chemically resistant but expensive and sticky; SEBS-based is cheap and soft to the touch — mainstream handles are SEBS-based.

High-end chemical-resistant silicone composite, conventional SEBS-based — choose according to positioning.

Two pitfalls: material too soft, chemically falsifiable

Pitfall 1: The material is too soft. If it feels sticky when drawn and the handle is hard to hold, it's too soft—balance between softness and hardness should be included in the acceptance criteria.

Pitfall 2: Falsely claiming chemical resistance. The report states chemical resistance, but in reality it corrodes — chemical resistance should be accepted based on actual testing.

Pitfall 3: Ignoring precipitation. High-temperature precipitation, handle becomes sticky — precipitation testing, must be tested.

Chemical Resistance Acceptance: Soaking Solution, Drawing, Delamination

Three questions: What sample is the texture benchmarked against, what medium is used for chemical resistance, and what is the range of hardness? One test: actual measurement of grip—three questions and one test make the supplier's details clear.

Hardness testing should come first: if the wire drawing keeps breaking, the material may be too soft. Test the hardness window first, then discuss the feel—hardness is the skeleton of the handle.

Making sample retention a habit: retain samples for each batch, and test them batch by batch for tactile and chemical resistance. When changing materials for a batch, compare first before scaling up — stable batches lead to fewer customer complaints.

Don't blame the process for the handle brushing first. The material is too soft, and once the mold temperature rises, it will stick and cause threads during demolding. Check both the hardness of the formula and the mold temperature, increase the hardness by one level, and the threads will break cleanly.

Resistance to chemicals is based on soaking in a 'mixed medium,' not a single emulsion. Essences and makeup removers are applied alternately, and with high temperatures, passing at room temperature does not mean it will still pass an hour later when held in hand.

Low-saturation, pearlescent colors are extremely picky about the base color; if the substrate is slightly yellow, no color can be adjusted correctly. First, print the color card to confirm the base color before discussing mass production. Low-cost materials have many impurities, and the yield of color spots cannot be improved.

The number of surface impurities must strictly adhere to the standard. Beauty devices that are applied to the face and hands, any rough edges, logo bubbles, or color spots are flaws that reduce the sense of high-end quality, which can only be achieved with pure base materials.

The material of the beauty device handle is a 'detail-oriented type': if the feel is slightly off, the sense of high-end quality drops a level. Lotion is most active and most corrosive at body temperature, so choose the material based on operating conditions, not room temperature.

Key Points Checklist for Acceptance of Beauty Device Handles

ProjectTest methodPassing line
Chemical-resistantSoaking in mixed mediaCorrosion-free
BrushedDemolding visual inspectionNo brushing
PrecipitationLeft at high temperatureSurface is clean
Surface qualityNumber of impurities≤ Standard
BatchThree rounds of random inspectionsData consistency

Common Problems and Solutions Table for Beauty Device Handles

PhenomenonReasonCountermeasure
BrushedThe material is relatively softIncrease hardness
stickyMedia corrosionReplace chemical-resistant material
DelaminationParameter OffsetAdjust mold temperature and maintain pressure
Deckle edgeMold wearMold repair
colored dotBase material impuritiesChange to a pure base material

If the handle of the beauty device keeps getting stringing, first check if the material is too soft; it is not a mold problem. Soft material sticks to the mold and causes stringing, and when workers try to pry it off with a blade, the production is halved. Increasing the hardness by half a grade usually solves the problem.

The handle is skin-friendly, with a Shore A 30-40 softness, soft and smooth like a pacifier, making it skin-friendly. Sticky exudation on contact with the face looks cheap, so a low-migration formula with low-exudation oil is used.

The adhesion strength of the coated material is assessed based on long-term gripping tests; it only counts if it does not come off after sweat immersion. It cannot be pried off with nails or crack when bent, and the data follows batch submission.

Cologne Customer Case: Bulk delamination of overmolding, replicated according to production benchmarks

At an electronics consumer factory in Ma'anshan, the coating on the handles of beauty devices was delaminating in large quantities, and the rework rate remained high. Kolon cooperated on-site during production debugging until the yield stabilized, and the tactile rebound was reproduced to match the sample. During production debugging, the delamination was stopped at its source—the coating issue, which in most cases was due to not finding the correct window for temperature and pressure.

Summary

When selecting a beauty device handle, first balance softness and hardness, then test chemical resistance, ensure it doesn't break under brushing, and let the formula decide.