工具防滑垫用什么TPE?变黄有规律,UV剂量说了算

应用领域 发布时间: 2026-09-15 1676 阅读

The anti-slip tool mat turned yellow and sticky after being exposed to the sun for two months, leaving a layer of oil on the countertop. The anti-slip tool mat was not chosen for sun resistance, and putting it down actually made it sticky to the touch.

After being exposed to the sun for two months, it turns yellow and sticky, and the countertop has a layer of oil.

Tool anti-slip mats are "components that provide anti-slip support": anti-slip, sun-resistant, wear-resistant. The material should be anti-slip, sun-resistant, and wear-resistant — conclusion first: SEBS-based TPE is the mainstream for tool anti-slip mats; for outdoor anti-slip mats, TPV is preferred.

The biggest pitfall of anti-slip tool mats: turning yellow follows a pattern, controlled by the UV dose. Once the UV dose reaches a certain level, yellowing is inevitable—the UV dose is the switch for yellowing.

Tool anti-slip mats are functional components: yellowing and cracking are problems. Choose the right material, and the tool will be stable—functional components are not the place to skimp on material costs.

Why use TPE for anti-slip mats

Reasons for using TPE for tool anti-slip mats: It can be made non-slip, it can be made sun-resistant, it can be made wear-resistant, and it is efficient—combined together, these four make it suitable for anti-slip mats.

Slip resistance is key: tools must be slip-resistant. Slip resistance tests should be included in the acceptance criteria—if it slips, it's a problem.

Sun resistance cannot be compromised: sun exposure causes yellowing. Sun resistance testing should be included in acceptance—yellowing is a problem.

Non-slip, resistant to sunlight and oil, three barriers

Anti-slip condition: Tool anti-slip. Anti-slip data must be verified—slipping is a problem.

Sun exposure condition: Yellowing under sun exposure. Sun resistance data needs to be checked—yellowing is a problem.

Oily condition: Contact with oil. Oil resistance data needs to be tested—swelling is the problem.

SEBS base or TPV? Anti-slip mat comparison

DimensionSEBS baseTPV
Non-slipCan be doneGood
Sun-resistantCan doGood
Wear-resistantmiddleGood
CostmiddleMedium-high
Oil-resistantCan be doneGood
PurposeIndoorOutdoor

Table interpretation: TPV is resistant to sunlight and oil, but expensive; SEBS has a high cost-performance ratio — indoor anti-slip mats are made of SEBS, outdoor ones of TPV.

Choose according to the environment: outdoor TPV, indoor SEBS base.

Anti-slip mat inspection: yellowing check UV dosage

IrradiateTurn yellowJudgment
500hSlightly yellowQualified
800hLight yellowFollow
1000hyellowBe alert
1500hDeep yellowMaterial change

Table reading: UV is measured level by level, yellowing is visible — only when the xenon lamp has aged for the specified time and the color difference ΔE does not exceed the standard is it approved.

UV dosage is the switch for yellowing.

Only check the material, not the UV, three pitfalls

Pitfall 1: Only check the materials, not the UV. If it yellows after being outdoors for a month, it means the UV dosage wasn't controlled — UV must be checked.

Pitfall 2: Missed UV testing. Cracking — UV resistance testing is a must.

Pitfall 3: Misleading anti-slip claims. Slipping — anti-slip should be verified according to actual measurements.

Check the UV dose first when choosing an anti-slip mat

Three questions: indoor or outdoor, UV for how many hours, anti-slip according to which surface. One test: actual use and measurements — three questions and one test, the supplier's details are clear.

UV testing must come first: first do xenon lamp aging and color difference tests before determining the weather resistance level. Check UV first, then talk about price—the UV dose is the switch for yellowing.

Making sample retention a habit: retain samples for each batch, and retest slip resistance and sun resistance batch by batch. When changing materials between batches, compare first before scaling up — stable batches result in fewer customer complaints.

Tool anti-slip mat: Follow this chart to avoid pitfalls

PhenomenonReasonCountermeasure
Turn yellowInsufficient UVAdd UV inhibitor
slipInsufficient slip resistanceReplace the anti-slip material
CrackingInsufficient sun resistanceChange to sunscreen-resistant material
SwellingInsufficient oil resistanceReplace with oil-resistant material
Batch DriftFormula fluctuationLock window

The mainstream anti-slip mat is SEBS-based TPE, Shore A 60-75. Once the UV dose reaches the point where it turns yellow, it can't be avoided. The yellowing follows a pattern, and only a complete anti-aging system (UV absorber, antioxidant, stabilizer) can withstand sun exposure.

SEBS is used indoors for slip resistance, TPV is used outdoors for weather resistance and sun exposure. Indoor workshop uses SEBS, outdoor workstations use TPV — choose the system according to sun exposure.

If the anti-slip mat turns yellow, first check the UV dosage and the anti-aging system, don't blame the substrate. If one stabilizer is missing, it will yellow first—have the supplier explain the system before accepting it.

Anti-slip mat inspection: three tests of UV aging resistance, anti-slip friction, and oil immersion resistance. Surface patterns are designed according to use, and swelling tests are performed separately for oily environments.

Switch the system to lock the dimensions, and the customer continued to place reorder for three consecutive batches, so the anti-slip mats no longer fluctuate in volume. Keep samples from each batch to test sun resistance and anti-slip properties; when changing materials for a batch, compare first before scaling up.

Choose anti-slip mats according to sun exposure: SEBS for indoor workshop use, TPV for outdoor stations. SEBS is for indoor anti-slip traffic, TPV is for outdoor weather resistance and sun exposure. If it yellows, first check the UV dosage and the anti-aging system; don't blame the base material. If any stabilizer is missing, it will yellow first.

Test UV aging resistance and oil immersion resistance together in three stages. Surface texture is designed according to its use. In oily environments, conduct swelling tests separately. Keep samples from each batch to test sun resistance and anti-slip properties.

The surface texture is designed according to use, and in oily environments, a separate swelling test is conducted. Samples are kept from each batch to test for UV resistance and slip resistance; if any stabilizer is missing, yellowing occurs first, and the UV dosage determines the outcome.

Tool anti-slip mats turn yellow, UV dose determines it. For indoor SEBS and outdoor workstation TPV in the workshop, select according to sunlight exposure, with three checks for sun resistance: UV aging, oil soaking, and surface texture designed according to use; oil stains are tested by swelling.

Each batch of samples is sun-resistant and anti-slip.

For each batch of anti-slip mats, samples are kept to test sun resistance and anti-slip properties. In oily environments, swelling tests are conducted separately. Yellowing follows the UV exposure dosage; if stabilizers are lacking, yellowing occurs first. Surface patterns are designed according to usage, with separate systems for indoor and outdoor applications.

Cologne Customer Case: Unstable shrinkage and size fluctuations, continued three orders after changing the system

A hardware tool factory in Jinhua had inconsistent shrinkage rates for its non-slip tool mats, resulting in significant size fluctuations. Kolon helped by changing the system and switching grades (from SEBS-based to TPV-based), stabilizing the dimensions, and the customer consecutively reordered for three batches. By changing the system, the size problem was addressed at the source — first check the system stability to solve shrinkage issues.

Summary

For selecting non-slip tool mats, first check UV resistance, then test slip resistance. To prevent yellowing, follow the UV dosage rules; UV acts as a switch.

For more than ten years, we’ve only done one thing: make nylon usable.

PA6 and PA66 are the basics, PA46, PA6T, PA9T are the thresholds for high temperature resistance, PA11 and PA12 manage water and oil circuits, and nylon alloys balance what a single resin cannot. Modified thermoplastic elastomers, modified nylon, modified PPO, PPS run in parallel, along with major chemical companies’ nylon resins, alternate brands, and bulk material in stock.

Using the same material in the wrong place causes accidents. So first ask about the part, then about the material.

这台机器上的件,说下工况我帮你看看

报个件、说清温度和要过的认证,当天回你两三个能打的方案。电话微信同号,找到人就能聊。

打电话 18969817163发邮件询价