食品密封圈用什么材料?耐候三年和五年,价格差15%

应用领域 发布时间: 2026-09-13 2824 阅读

The sealing ring becomes sticky and cracks after two years, and the customer says it is not weather-resistant. The lifespan of outdoor food parts was not calculated clearly, and the money saved is not enough to cover the losses.

Sticky and cracking is not because it's old, but because the weather resistance was not chosen enough.

Food sealing rings are 'sealing and weather-resistant components': weather resistance, sealing, migration. The material must have weather resistance, sealing, and migration—conclusion first: SEBS-based TPE is mainstream for food sealing rings; for long-term outdoor use, TPV is preferred.

The biggest pitfall of food sealing rings: they claim to be weather-resistant for three years or five years, with a 15% price difference. A difference of two years in weather resistance results in a significant price gap—weather resistance years are the price line for sealing rings.

Food sealing rings are food parts: aging and leakage are both problems. Choosing the right material ensures food safety—don't skimp on material costs for food parts.

Exposed to sun and rain outdoors, why choose TPV weather-resistant material

Reasons for using TPE for food sealing rings: weather resistance can be achieved, sealing can be achieved, migration can be controlled, efficiency is high—combined, these four points make it suitable for sealing rings.

Weather resistance is key: long-term use. Weather resistance testing is written into acceptance — aging is the problem.

Sealing cannot be overlooked: leak-proof sealing. Include sealing tests in acceptance inspections—any leakage is a problem.

Sealing, weather resistance, contact—what to check in each of the three areas

Sealing conditions: Leak-proof sealing. Sealing data must be verified—leakage indicates a problem.

Weather-resistant conditions: long-term use. Weathering data must be verified — aging is the problem.

Contact condition: in contact with food. Migration data must be tested — if it exceeds the standard, it's a problem.

SEBS vs TPV, which one is chosen in the food industry

DimensionSEBS-based TPETPV
weather-resistantCan doGood
SealCan doGood
MigrationControllableControllable
CostmiddleMedium-high
Lifespan3 years5 years
PurposeRegularLong-term

Table reading: TPV has good weather resistance but is expensive; SEBS is cost-effective - conventional seals are SEBS-based, long-term use is TPV.

Select by duration: long-term TPV, conventional SEBS base.

Does not crack or become sticky when dried; check these four items during inspection

Years of servicePriceJudgment
3 yearsBenchmarkMeet the standard
4 years8%Follow
5 years15%Meet the standard
6 years22%Over-allocation

Table reading method: Determine the weather resistance years according to the shelf life; if the resin can last two more years, it moves up a grade—the difference between three years and five years is one grade, and the unit price differs accordingly.

Service life is the price benchmark for gaskets.

Only looking at the price without considering the age, it becomes unusable in just two years

Pitfall 1: Only looking at the price. Choosing a short-term option, the shelf cracks before its lifespan ends — set the seal replacement schedule according to the actual replacement cycle, neither over-supplying nor under-supplying.

Pitfall 2: Missed migration testing. Exceeding the limit — migration testing is mandatory.

Pitfall 3: Seal leakage testing. Leakage—seal testing must be performed.

Service life, sealing, batch — ask clearly before setting the ring

Three questions: How many years for weather resistance, what standards for migration, what tests for sealing. One verification: actual measurement in use — three questions and one verification, the supplier's details are clear.

Weather resistance verification comes first: set the accelerated aging duration according to the product's shelf life, and only when the years match can the price be discussed. First determine the years, then discuss the price — the weather resistance period is the price line for sealing rings.

Making sample retention a habit: retain samples for each batch, and reseal them for periodic testing. When changing materials between batches, compare first before scaling up—the batch remains stable, and customer complaints are fewer.

Sticky, Cracked, Leaking: A Fault Comparison Table

PhenomenonReasonCountermeasure
AgingInsufficient weather resistanceReplace with weather-resistant material
LeakageInsufficient sealingReplace with high-density sealant
OdorAdditive precipitationSwitch to low precipitation material
TransformationInsufficient temperature resistanceChange to heat-resistant material
UnverifiedCertificate missingNuclear Certification

If the compression of the food sealing ring increases by more than 30% (70°C × 22h), it cannot rely on long-term sealing. Repeated opening and closing, hot soup, and hot water will cause leaks if the rebound fails; migration tests are classified according to oil, acid, and alcohol.

The service life is set according to the shelf life, neither over-specifying nor under-specifying. Holding on for a couple more years allows the resin to upgrade, with the unit price rising accordingly; the sealing ring can be recycled without vulcanization, saving a process compared to rubber.

Acceptance is all-or-nothing: sealing pressure test, migration, aging, and temperature resistance; if any item fails, it is not released. The numbers on the physical property table are typical, not the minimum; the minimum is written into the acceptance criteria. Samples are retested for each batch.

The sealing ring becomes aged and brittle, which is not normal wear from use, but because the temperature resistance grade wasn't selected correctly. For high-temperature conditions with hot dishes and soups, choose high-temperature resistant SEBS/TPV; excessive migration is mostly due to over-filling with oil, so switch to a low-exudation formula.

After switching to a low-extractable formula, migration testing after 90 days showed zero exceedances. Food contact reports are checked by batch; if batch hardness is within ±3A, customers cannot feel any difference between the two batches.

The food sealing ring soaks in the contents every day. The TPE must be food-grade, have low compression set, and be oil and acid resistant. If compressed for a long time and it doesn't rebound, it will leak flavor. Choose food-grade SEBS base, compliant with GB4806 and LFGB; leave a compression of 15%-25%, compression set after 70°C × 22h is less than 30%, and fit with the groove.

Food item acceptance should be based on migration and batch, not on the feel of the new material.

Color masterbatch and additives must all be food-grade; migration exceeding the limit is more dangerous than the base material. Keep samples from each batch to test soaking liquid and hardness, and when changing materials, first test a small batch on the filling machine for leaks.

Food sealing ring final acceptance: Compression set, migration, and leakage test are conducted with each batch. For each batch, samples are kept to measure compression set and migration in soak solution at 70℃ × 22h, not exceeding limits; when changing material for a batch, a small batch is tested on the filling machine for leakage, and only if there is no seepage is it released.

When it comes to selecting food sealing rings, it ultimately comes down to asking about three things at once: compression set, migration, and leak testing. Food-grade SEBS meets GB4806 standards, with a compression set below 30% and migration limits not exceeded; first, conduct leak tests on a small batch filling machine, and only release if there is no leakage.

Cologne Customer Case: Flame Retardant Failed Inspection, Export Blocked, Reformulated to Pass Inspection

A car parts factory in Huizhou faced a problem where food-grade sealing rings failed the flame retardancy test, causing export issues. Cologne assisted in readjusting the formula (oil/additive/filler ratio), allowing the flame retardancy to pass and the products to be exported smoothly. When the formula is readjusted, passing the flame retardancy stage is about the formula — for flame retardancy issues, start by looking at the additive system.

Summary

For selecting food-grade sealing rings, first determine weather resistance, then test sealing performance. The price difference between three-year and five-year weather resistance is 15%, with the weather resistance period determining the price line.

这台机器上的件,说下工况我帮你看看

报个件、说清温度和要过的认证,当天回你两三个能打的方案。电话微信同号,找到人就能聊。

打电话 18969817163发邮件询价
WA