继电器与线圈骨架用尼龙?耐温、绝缘、薄壁都缺一不可

应用领域 发布时间: 2026-09-16 2240 阅读

Relays and coil cores belong to the type of components that 'look insignificant but can cause serious problems if they fail.'

It does not bear heavy loads or show any external appearance, but it keeps the wires and contacts fixed in an exact position. Once it softens and deforms, suffers creepage breakdown, or the terminals crack, the whole device fails.

Choosing the material for the frame is essentially about finding a balance between temperature resistance, insulation, thin-wall forming, and insert strength.

The failure of relay frameworks mostly occurs in areas that are not visible to the customer.

When the coil is energized and generates heat, the framework remains in a temperature-rise environment for a long time, causing the insulation resistance to slowly decrease.

In the after-sales data of a relay factory, repairs due to parameter drift accounted for the majority of complaints.

Upon inspection, the framework has not deformed or cracked; only the dielectric properties have quietly deteriorated.

This kind of silent failure is the hardest to prevent and also the most challenging test of foresight in material selection.

1. Coil temperature is the first variable

The frame is closely attached to the coil, and it is exposed to the winding temperature rise environment for a long time.

Insulation class and temperature rise correspond as follows: Class B corresponds to about 130℃, Class F to about 155℃, and Class H to about 180℃. The temperature here refers to long-term continuous temperature rise, not short-term peaks.

The first step in material selection is not to ask 'how much temperature it can withstand,' but to clarify the insulation class of the coil and the actual measured temperature rise.

Just one grade difference, and the material direction is completely different: at 130℃, flame-retardant reinforced PA66 can be used; at 155℃, a high-temperature system or PA46 is often needed; above 180℃, usually PA6T, PA9T, or PPS at this level must be considered.

It is also necessary to distinguish between two types of temperatures: the temperature inside the winding is usually higher than the surface, while the frame is in close contact with the winding. Therefore, the location of the measurement point is very important; using the casing temperature instead of the winding temperature will underestimate the requirements.

A prudent approach is to ask the customer to provide the measured temperature rise curve of the winding, looking at the steady-state value rather than the peak value at a particular moment.

2. Thin walls with inserts are the structural destiny of the framework.

The typical characteristics of the skeleton are: the walls are very thin, the dimensions are very tight, and the terminals are embedded inside.

The difficulty with thin-walled parts lies in the flow — the process is long, the wall is thin, and the area around the terminals must also be filled. If the material's fluidity is insufficient, it will result in incomplete filling or weak weld lines.

The difficulty with inserts lies in stress—the metal terminals and plastic have different thermal expansions, and when cooling, the plastic shrinkage is constrained by the metal, forming a ring of stress concentration around the terminals.

When two difficulties overlap, the result is often microcracks near the terminals. This type of problem is often not detectable during factory inspection and only becomes apparent after installation, soldering, or several thermal cycles.

The sequence of countermeasures is: first add fillets and interlocking structures to the terminals, then try preheating the inserts, and only finally consider changing the material.

There is another detail that is easily overlooked: the thickness of the plastic between the terminal and the hole wall. This thickness determines the plastic's ability to constrain the metal; if it is too thin, the metal will 'bite' and cause stress concentration, and if it is too thick, it will make the terminal loose.

It is generally recommended that the thickness of the hole wall be kept in a certain ratio to the diameter of the terminal, while leaving a transition fillet at the hole opening. These two points are related to design standards and are decided earlier than material selection in determining success or failure.

3. The creepage distance is the "invisible dimension" of the framework

The geometric shape of the skeleton is often the physical carrier of the product's creepage distance.

The distance of the plastic surface between two charged parts directly determines how high a voltage the product can withstand and what level of safety standard it can meet.

This matter is often regarded purely as a structural problem, but in fact it is determined by both materials and structure: for the same distance, high CTI materials can withstand higher voltage; conversely, using high CTI materials allows the distance to be shortened and the product to be made smaller.

The relay voltage levels of new energy platforms are higher. The CTI and arc resistance requirements for the frameworks of 400V and 800V platforms are much stricter than traditional 12V and 24V systems, and using old brands often cannot pass the new tests.

4. Correspondence Between Material Grades and Temperature

Long-term temperature riseMaterial directionRemarks
Within 130℃Flame-retardant reinforced PA66The cost and technology are the most mature
About 155℃High-temperature system PA66 / PA46Need to confirm long-term thermal aging data
Above 180℃PA6T / PA9T / PPSThe process window varies greatly and needs to be adjusted simultaneously.

Pay attention to the last line: the material temperature, mold temperature, and drying conditions for high-temperature nylon are completely different from PA66; changing the material without changing the process is equivalent to changing for nothing.

There is another question that is often asked when selecting materials: whether PPS can replace high-temperature nylon. The main differences between the two are in process and cost: PPS has extremely low water absorption and more stable dimensions, but it has poor toughness, high molding temperature, and high requirements for molds; high-temperature nylon has better toughness, the process is closer to PA66, and the modification cost is low.

The way to judge is by looking at the shape of the framework — for thin-walled, long-process, complex structures, high-temperature nylon is easier to use; for flat types with extremely stable size requirements, PPS has more obvious advantages.

No matter which one is chosen, the terminal insert scheme must be recalculated: with different materials, both the shrinkage rate and the thermal expansion coefficient change, and the original interference fit is no longer applicable.

There's one more point that's easily overlooked: the storage and humidity adjustment of the skeleton. The size and toughness of high-temperature nylon will change after absorbing moisture, and if the customer only unpacks it before assembly, the dimensions may have already shifted. Whether to adjust humidity, when to adjust it, and at what moisture content to deliver should all be written into the supply agreement.

5. The three things a skeleton fears the most

First, there is insufficient filling. The long thin-walled process cannot be completely filled, resulting in material shortages around the terminals.

Secondly, the weld line falls on a stressed or weak insulation area. The strength of the weld line in fiberglass materials is low, so the gate location must avoid these areas.

Third is the dimensional drift after water absorption. The positioning dimensions of the framework are usually very tight, and moisture-induced expansion can make the assembly tighter or looser.

None of these three issues can be solved simply by 'changing to better material'; it requires a combination of gate design, mold temperature control, drying, and post-processing.

6. The process window cannot be copied directly

On the same injection molding machine, when switching from PA66 to PA6T, it is necessary to adjust the material temperature, mold temperature, injection speed, holding pressure, and drying conditions simultaneously.

Thin-walled precision parts like skeletons are particularly sensitive to mold temperature—if the mold temperature is insufficient, both flow and crystallization are suboptimal, and the dimensions deteriorate along with the weld lines.

"The same grade, but two manufacturers produce different results" is particularly evident in the framework, because the process window is narrow, and even a slight deviation leads to different outcomes.

7. Verification Checklist

It is recommended to test these five items before sending the sample:

① Voltage resistance and insulation resistance, and they should be measured in a humidity-controlled state.

② CTI also needs to adjust the wet-state data.

③ Ball pressure, confirm that it does not soften under long-term temperature rise.

④ Terminal pull-out force, used to measure the bonding strength of the insert.

⑤ After thermal cycling, retest the first four items to see if there is any degradation.

These five items are not complicated, but they can cover the vast majority of failure modes of the framework.

The insulation deterioration of the skeleton should be thoroughly explained in terms of mechanism.

The coil temperature rise keeps the skeleton at 80 or 90 degrees or even higher for a long time.

PA dielectric performance declines with both temperature and moisture absorption lines, making the overlap even more pronounced.

When the coil is energized, it generates an electric field, and partial discharge slowly accumulates damage at weak points.

So the skeleton material should be based on the dielectric data at three temperature points, not just one point at room temperature.

In the hot and humid southern market, the moisture absorption line must be strictly enhanced.

Some factories supply by sales region, but the southern market uses low moisture absorption grades.

Regional selection sounds troublesome, but the after-sales data is very honest.

Follow-up question 1: How often should the insulation resistance of the skeleton be measured?

Factory full testing, durability sampling by batch. The dielectric decay of the skeleton is a slow variable; batch sampling and periodic durability are two lines. During hot and humid seasons, the frequency of sampling is increased; skeleton materials in southern warehouses are recommended to be managed at low moisture absorption levels.

Follow-up question 2: How is the temperature resistance of coil skeleton graded?

Set it as the sum of temperature rise and ambient temperature, leaving a one-tenth margin. If the relay's internal cavity temperature is tens of degrees higher than the ambient temperature, the skeleton grade should be calculated according to the internal cavity, not by the environment. This difference is a miscalculated error and is the most common error in skeleton selection.

Tracking parameter drift in a single order

A relay batch has parameter drift, rework parts disassembled and the skeleton is intact. Finally, the focus is on moisture absorption: after three months of storage in the south, the skeleton moisture content increased, the dielectric constant drifted, and the coil inductance changed accordingly. Rectification involves dehumidifying the warehouse and selecting a low moisture-absorbing grade. For difficult problems like parameter drift, the answer often lies in the most basic physical knowledge.

Three looks at skeleton selection

Check the temperature point dielectric data, see the moisture absorption level matches the sales area, and check thin-wall flow and forming accuracy. Third, check completely, and the bottom line of the skeleton performance is clear.

To conclude: The relay is the sentinel of the electronic system, the skeleton is the armor of the sentinel. Armor may not be loud or flashy, but half of the sentinel's reliability rests on it. When selecting materials, one more look at the temperature and humidity hyperbola makes the client's equipment more stable.

Relay Framework has an extended topic: the differentiation between signal relays and power relays. Signal relays pursue reliable contact, while the skeleton requires the ultimate in dielectric; Power relays pursue current carrying and the skeleton demands extreme temperature resistance. Within the same family, two technical routes have completely different material selection logic. Supporting factories build two material lists according to the route, which is clearer than covering everything in one list. The more segmented the industry, the more the material list must be divided. Factories that treat a universal material list as a family heirloom cannot take orders from a niche market. The mold precision of

skeleton is also worth mentioning. The skeleton is a thin-walled part, and the core is slender; the melt erodes the core and its offset directly affects wall thickness uniformity. For a skeleton with uneven wall thickness, the dielectric weak point is at the thinnest point. Mold venting, core positioning, and holding pressure setting determine wall thickness uniformity. When selecting materials, choose grades with stable flow to reduce the risk of core misalignment. Material flow stability is not an indicator on physical property tables, but it appears in the actual tests of every batch of skeletons. It needs trial production data to speak for itself, and suppliers need to be willing to accompany you through trial production.

List End

Relay Framework Fixed Point Data Package: Three temperature point dielectric data, moisture absorption level and area matching, thin-wall trial production wall thickness uniformity, insulation retesting after aging, compatibility with paint or encapsulation materials. Although the skeleton is small, the thickness of the data package determines the depth of cooperation.

There is another detail in the encapsulation collaboration of the relay skeleton. Some relay processes install the skeleton first and then apply glue for encapsulation; the adhesive cures and shrinks to pull the skeleton outward. The thermal expansion coefficient between the skeleton and the glue is very different, and the stress at the interface during temperature cycling repeatedly pulls and tugs at the interface. Some factories have skeleton cracks during low-temperature periods, and it is found that the glue formula has been replaced with hard glue. Change management of the encapsulation system requires skeleton re-testing into the process. The glue and skeleton are like two grasshoppers tied to the same rope; the movement of one end must be known at the other. The assembly precision of the

skeleton is also worth mentioning. The moving contact spring presses against the skeleton, and the spring pressure acts long-term on the thin-walled cantilever of the skeleton. The creep of the cantilever causes contact pressure to decay year by year, causing key relay parameters to drift along with it. When selecting materials, creep modulus is the number one indicator for the skeleton, even ahead of strength. Some relay factories include five-year contact pressure attenuation values in their selection specifications, making supplier creep data a mandatory item in the quotation. One parameter controls one class of parts; with each additional refinement, the supply chain stabilizes.

Advice for New Procurement Professionals: When evaluating skeleton components, focus on three key factors—completeness of dielectric testing equipment, completeness of temperature and humidity hyperbola data, and willingness to cooperate in trial production. All three are slow processes and can't be assembled. It took three batches of suppliers to find the right factory for frame parts, and the common point is that all three are present.

Relay Components also have a new requirement for automated assembly. Automated production lines demand extremely high dimensional consistency for the skeleton; deviations tolerated in the manual assembly era are not tolerated by robotic arms. As a result, the molding stability of skeleton materials has been elevated to a new level. Some factories have automated modifications stuck on skeleton feeding, causing dimensional fluctuations to cause excessive failure rates in robotic arm grasping. Ultimately, this is resolved by switching to stable grades and process optimization. The automation wave has raised the tolerance requirements for plastic parts by a notch, and the material side must keep up.

Skeleton marking management is also worth mentioning. There are many relay models, and the skeleton must have model markings and be made together during injection molding. The clarity of the labels affects downstream assembly efficiency, and the height and depth of the text are all carefully considered. Maintenance cycles for mold fonts must be included in the maintenance plan, and worn letters cause frequent shutdowns on the production line. Even a single line of text is behind the efficiency account.

's final advice for relay manufacturers: When evaluating skeleton materials, prioritize molding stability first, dielectric data second, and price third. Materials with unstable molding won't withstand the test of automated production lines no matter how good the dielectric is. If the order is right, the selection process will be faster.

Conclusion

Relay skeleton material selection, the judgment chain is:

First determine coil temperature rise and insulation grade→ then set creepage distance and CTI →, then decide on thin-walled and insert forming schemes→ finally decide on materials.

The order is correct, the material selection step is very short; If the order is wrong, every subsequent step must pay for the previous one.

We stand between the resin plant and the injection molding plant

这台机器上的件,说下工况我帮你看看

报个件、说清温度和要过的认证,当天回你两三个能打的方案。电话微信同号,找到人就能聊。

打电话 18969817163发邮件询价
WA